COMPOSITION
It consists of two components, A is polyol and B is prepolymer.
CHARACTERISTICS
Good processing, blending and casting in room temperature with short demould time, suits for production line.
APPLICATION
It applies to make insole, non-slip mat, heel cushion, low hardness gel products etc.
PHYSICAL PROPERTIES
Type |
DX1615-A |
DX1660-B |
|
Appearance |
pale purplish transparent colorless liquid |
Colorless transparent liquid |
|
Ratio A:B(mass ratio) |
100:33~38 |
||
Operating temperature(℃) |
30~40 |
30~40 |
|
Mould temperature(℃) |
70~90 |
||
Gel time(sec/80℃)* |
40~50 sec |
||
Demould time(min/80℃) |
3~5 min |
||
Appearance of ware |
Colorless transparent elastomer |
||
Hardness of ware(Shore O) |
40~60 |
||
Tensile strength (Mpa) |
1.0~1.5 |
||
Ultimate elongation (%) |
800-1000 |
||
Special gravity |
1.05 |