INTRODUCTION
DonPanel 203 blend polyols is a compound which consists of polyether polyols, surfactants, catalysts and so on in a special ratio. The foam has good thermal insulation property, light in weight, and other advantages. It is widely used in solar water heater.
PHYSICAL PROPERTY
Appearance | Light yellow transparent viscous liquid |
Hydroxyl value mgKOH/g | 300-400 |
Dynamic viscosity ( 25℃) mPa.S | 300-500 |
Density ( 20℃) g/ml | 1.02-1.07 |
Storage temperature ℃ | 10-20 |
Storage stability month | 6 |
RECOMMENDED RATIO
Raw materials | pbw |
blend polyols | 100 |
Isocyanate | 115-125 |
Technology and Reactivity (the exact value varies depending on processing conditions)
items | Manual mixing | High Pressure Machine |
Raw material temperature ℃ | 20-25 | 20-25 |
Cream time s | 8-15 | 6-10 |
Gel time s | 70-85 | 50-65 |
Tack free time | 90-125 | 70-95 |
Free density kg/m3 | 28-30 | 27-29 |
FOAM PERFORMANCES
Moulding density | GB 6343 | ≥38kg/m3 |
Closed-cell rate | GB 10799 | ≥90% |
Thermal conductivity( 10℃) | GB 3399 | ≤0.019W/(m.K) |
Compression strength | GB/T 8813 | ≥140kPa |
Dimensional stability 24h -20℃ | GB/T 8811 | ≤1% |
24h 100℃ | ≤1% |
The data provided above are typical value, which are tested by our company. For our company's products, the data included in the law do not have any constraints.